o2

  • Hot

    DC53 STEEL

    In the case of proper heat treatment, the strength and toughness are excellent, and the high temperature tempering hardness can reach 62~63HRC.

    The toughness of DC53 is more prominent in cold work die steel, and the tools made of DC53 rarely show cracks and cracks, which greatly improves the service life.

    The residual stress after wire cutting is tempered at high temperature to reduce the residual stress. Therefore, cracks and deformation after online cutting of large molds and molds that require precision are suppressed.

    Email Details
  • 1.2842 blade steel

    1.2842 steel is cold work die steel is easy to forge and requires a hardness of 63HRC.

    chemical composition
    1.2842 chemical composition (mass fraction): C0.85% ~0.95%, Si0.10% ~0.40%, Mn1.90%~2.10%, P≤0.030%, S≤0.030%, Cr0.20% -0.50% , V0.05% ~0.15%.

    Reference corresponding grade
    Chinese GB standard grade 9Mn2V, international standard ISO grade 90MnV2, German DIN standard grade 90MnV8, German DIN standard material number 1.2842, American ASTM standard grade 02, British BS standard grade B02, Sweden ASSAB (ASSAB) standard grade DF- 20

    Email Details
  • 1.2842

    DIN 1.2842 90MnCrV8 steel is suitable for cutting and punching tools, little shear blades, thread cutting rings and jaws, reamers, measuring tools, sliders, rails, plastic and rubber molds.

    Email Details